Download PDF
Composition
Carbon, Hydrogen doping elements
Structure
Mixture of sp3 (tetrahedral diamond type) and sp2 (trigonal graphitic)
Coating Thickness
3.5 – 5.0 microns
Density
1.92-2.2 g/cm3
Hardness
3500-3900 HV (30-35 Gpa)
Co-efficient of friction
DiamondV® on Steel: 0.05 (Example:Steel on Steel-0.45)
Adherence Scratch test
LC=40 N
Thermal conductivity
>400 W/K/m
Coefficient of dilation
2.10-6/° C
Permeability Barrier
to hydrogen and other gases
Electrical resistivity
108 ohms cm
Chemical resistance
Inert in acids, alkalis, solvents, salts & water
Successfully Used on
Shaft,Stems,Bushing,Ball & Butterfly Valves
DiamondV offers the following advantages:
- Substantial torque reduction due to > 10 friction (metal on metal)
- Torque breakaway reduced by 30% to 40%
- No corrosion, sticking, media, wear or galling
- Ideal for gas, refractory, pulp and paper service
- Eliminates valve & packing leaking, torque increase due to premature wear
- Replace sellite with 316 S.S for bearing
- Extends valve life by 2 to 3 years and operate at tempature over 575 degree F
- Cost of ownership saving over 50% with substantial maintenance and spare inventory cost reductions